# Adsorbent Gas q / mol kg⁻¹ S / mol mol⁻¹ -ΔH / kJ mol⁻¹
685 ZIF-8 Carbon dioxide/Methane 0.57 2.61 None
686 ZIF-8 3 h - 25C (H2S exposure) Carbon dioxide/Methane 0.57 2.61 None
687 ZIF-8 3 hr - 75C (H2S exposure) Carbon dioxide/Methane 0.57 2.61 None
688 ZIF-8 10 h - 75C, (H2S exposure) Carbon dioxide/Methane 0.57 2.61 None
689 UiO-66-NH2 Carbon dioxide/Methane 1.72 2.75 None
690 UiO-66-NH2 3 h - 25C (H2S exposure) Carbon dioxide/Methane 1.72 2.75 None
691 UiO-66-NH2 3 hr - 75C (H2S exposure) Carbon dioxide/Methane 1.72 2.75 None
692 UiO-66-NH2 10 h - 75C, (H2S exposure) Carbon dioxide/Methane 1.72 2.75 None
693 PCN-250 Carbon dioxide/Methane 2.0 2.56 None
694 PCN-250 3 h - 25C (H2S exposure) Carbon dioxide/Methane 2.0 2.56 None
695 PCN-250 3 hr - 75C (H2S exposure) Carbon dioxide/Methane 2.0 2.56 None
696 PCN-250 10 h - 75C, (H2S exposure) Carbon dioxide/Methane 2.0 2.56 None
697 HKUST-1 Carbon dioxide/Methane 4.0 4.94 None
698 HKUST-1 3h-25C (H2S exposure) Carbon dioxide/Methane 0.57 3.06 None